Abstract

Purpose: The study determined (i) the effects of electrical discharge machining (EDM) on the shear-bond strength (SBS) of the bond between luting resin and zirconia ceramic and (ii) zirconia ceramic's flexural strength with the three-point bending (TPB) test. Methods: Sixty 4.8 mm x 4.8 mm x 3.2 mm zirconia specimens were fabricated and divided into four groups (n = 15): SBG: sandblasted + silane, TSCG: tribochemical silica coated + silane, LTG: Er:YAG laser treated + silane, EDMG: EDM + silane. The specimens were then bonded to a composite block with a dual-cure resin cement and thermal cycled (6000 times) prior to SBS testing. The SBS tests were performed in a universal testing machine. The SBS values were statistically analyzed using ANOVA and Tukey's test. To determine flexural strength, sixty zirconia specimens were prepared and assigned to the same groups (n = 15) mentioned earlier. After surface treatment TPB tests were performed in a universal testing machine (ISO 6872). The flexural strength values were statistically analyzed using ANOVA and Tukey's test (a = 0.05). Results: The bond strengths for the four test groups (mean SD; MPa) were as follows: SBG (Control), 12.73 +/- 3.41, TSCG, 14.99 +/- 3.14, LTG, 7.93 +/- 2.07, EDMG, 17.05 +/- 2.71. The bond strength of the EDMG was significantly higher than those of the SBG and LTG (p < 0.01). The average flexural strength values for the groups SBG (Control), TSCG, LTG and EDMG were 809.47, 800.47, 679.19 and 695.71 MPa, respectively (p > 0.05). Conclusions: The EDM process improved the SBS. In addition, there was no significant adverse effect of EDM on the flexural strength of zirconia.

Description

Keywords

Zirconia Ceramic, Electrical Discharge Machining, Bonding Strength, Flexural Strength, Graphite Powder

Turkish CoHE Thesis Center URL

Fields of Science

Citation

Rona, Nergiz...et.al. (2017). "Effect of electrical discharge machining on dental Y-TZP ceramic-resin bonding", Journal Of Prosthodontic Research, Vol.61, No.2, pp.158-167.

WoS Q

Scopus Q

Source

Journal Of Prosthodontic Research

Volume

61

Issue

2

Start Page

158

End Page

167